After the film is formed, stripes sometimes appear. The main reasons are:

(1) The quality of the paint is not good, the driers are too much, and the solvent evaporates too quickly.

(2) The paint mix is ​​uneven or too thick.

(3) The paint film is too thick and uneven.

(4) Construction under high temperature or sun exposure.

The following precautions can be taken:

(1) Do not add driers at will, and strictly control the consistency of the paint.

(2) Using a harder brush, brushing should be uniform and consistent in thickness.

(3) Avoid construction at high temperatures or in hot sun.